Ferromolybdeenin sulatusraaka-aineet

Raaka-aineita koskevat vaatimukset ovat seuraavat:
(1) Molybdeenin paahtaminen vaatii S<0.10%, Cu<0.6%, and Pb<0.5%. The actual ingredients are: Mo48.5%~52%, S0.04%~0.07%, P0.01%~0.02%, Cu0.1%~0.5%, Pb0.2%~0.5%, FeO3%~5%, SiO28%~14%, CaO2%~4.5%. 5% to 10% of the total molybdenum is in the form of MoO2, which should be considered when calculating the reaction heat. The particle size is <15mm, of which >10 mm on alle 10 % ja<2mm accounts for about 60%. (2) Ferrosilicon powder contains Si75%~77%; the particle size is <1mm.

 

Ferromolybdenum Block 60

ferromolybdeenijauheen hinta


(3) Aluminum particles contain Al>90 % ja Cu<0.1%; the particle size is <3mm, and the part <0.5mm shall not exceed 30%.
(4) Iron ore contains Fe>65%, S<0.05%, P<0.05%, C<0.30%; particle size<1mm. Iron oxide scale or iron concentrate can be used instead.
(5) Teräsromut ovat tavallisia hiiliteräsromuja, ja kiharan pituus on<50mm.
(6) Fluorite contains CaF2>90 %. Hiukkaskoko<3mm.

 

Molybdenum

Ferromolybdeenilejeeringin hinta


(7) Saltpeter contains NaNO3>90 %. Kaikki raaka-aineet on kuivattava perusteellisesti, eivätkä ne saa sisältää kosteutta roiskeiden ja onnettomuuksien välttämiseksi sulatuksen aikana. Raaka-aineet punnitaan tarkasti lasketun suhteen mukaan, laitetaan sekoittimeen ja sekoitetaan tasaiseksi, laitetaan sitten sulatusuuniin ja sulatetaan yläsytytysmenetelmällä.